Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 1.30 J | 0.959 ft-lb | ISO 6603-2 |
Lanxess Pocan® B 7616 000000 PBT + PC, 15% Glass Fiber PBT+PC, 15% glass fibers, injection molding, low tendency to warp, improved surface finish |
|||
Puncture Energy | 1.30 J | 0.959 ft-lb | 50 N; 40µm sample; ASTM D5748 |
Borealis FA6220 Low Density Polyethylene FA6220 is a Low Density Polyethylene for Film Extrusion. Includes Antioxidant. This grade is developed for the production of thin blown films. Applications: shrink film, pouches, general packagin.. |
|||
Puncture Energy | 1.30 J | 0.959 ft-lb | 50 N; 40µm sample; ASTM D5748 |
Borealis FA6224 Low Density Polyethylene FA6224 is a Low Density Polyethylene for Film Extrusion. Autoclave Technology. Contains Antioxidant, Anti-block and Medium Slip additives. This grade is developed for the production of thin blown f.. |