Mechanical Properties Metric English Comments
Puncture Energy 1.76 J
1.30 ft-lb
Exxon Mobil Method
ExxonMobil Exceed™ 1023DA Tough Premium Film Resin  (discontinued **)
Exceed 1023DA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1023DA resin have outstanding tensile, impact strength and puncture. These superi..
Puncture Energy 1.76 - 5.84 J
1.30 - 4.31 ft-lb
Average value: 4.08 J Grade Count:3
Overview of materials for Very Low Density Polyethylene (VLDPE)
This property data is a summary of similar materials in the MatWeb database for the category "Very Low Density Polyethylene (VLDPE)". Each property range of values reported is minimum and maximum va..