Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 17.0 J
12.5 ft-lb
Conditioned; ISO 6603-2
Lanxess Durethan® BKV 130 H2.0 901510 Copolyamide, 30% Glass Fiber
CoPA, injection molding grade, 30% glass fibers, elastomer-modified, electroplateable, improved notched impact strength and energy absorption under biaxial impact load, good heat-ageing resistance