Mechanical Properties Metric English Comments
Puncture Energy 3.16 J
2.33 ft-lb
ExxonMobil Method
ExxonMobil LDPE LD 331.08 Low Density Polyethylene Resin
Product Description: LD 331.08 is a 5.9% vinyl acetate copolymer, higher clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Availability: Latin Amer..
Puncture Energy 3.16 J
2.33 ft-lb
ExxonMobil
ExxonMobil LL 1001x26 Blown Film Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Puncture Energy 3.16 J
2.33 ft-lb
ExxonMobil Method
ExxonMobil LLDPE LL 1001X26 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Puncture Energy 3.16 J
2.33 ft-lb
ExxonMobil Method
ExxonMobil LLDPE LL 1001X31 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Puncture Energy 3.16 J
2.33 ft-lb
ExxonMobil Method
ExxonMobil LLDPE LL 1001X72 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Puncture Energy 3.16 J
2.33 ft-lb
ExxonMobil Method
ExxonMobil LLDPE LL 1001X74 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Puncture Energy 3.16 J
2.33 ft-lb
ExxonMobil Method
ExxonMobil LLDPE LL 1001X76 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Puncture Energy 3.16 J
2.33 ft-lb
Dow Method
Dow TUFLIN™ HS-7021 NT 7 Linear Low Density Polyethylene Resin
Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HS-7021 NT 7 is an ethylene-hexene-1 copolymer designed..
Puncture Energy 3.16 J
2.33 ft-lb
Dow Method
Dow TUFLIN™ HS-7094 NT 7 Linear Low Density Polyethylene Resin
Hexene Linear Low Density Resin Good Processability at Narrow Die Gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7094 NT 7 is a fractional melt, ethylene-hexene copolymer, designe..