Mechanical Properties Metric English Comments
Puncture Energy 2.10 - 3.50 J
1.55 - 2.58 ft-lb
Average value: 2.50 J Grade Count:5
Overview of materials for PBT + PET Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of ..