Polymer Property : Puncture Energy = 2.70 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 2.70 J
1.99 ft-lb
ISO 6603-2
Lanxess Durethan® DP AKV 30 HR EF 901510 Nylon 66, 30% Glass Fiber
PA 66, injection molding grade, 30% glass fibers, good heat-ageing resistance and hydrolysis resistance, good flowability (Easy Flow)
Puncture Energy 2.70 J
1.99 ft-lb
ISO 6603-2
Lanxess Pocan® TS 3220 901510 PBT + PET, 20% Glass Fiber
PBT+PET, 20% glass fibers, injection molding, impact modified, low tendency to warp, improved surface finish