Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 3.73 J | 2.75 ft-lb | ExxonMobil Method |
ExxonMobil Enable™ 20-05CH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 20-05CH is a metallocene ethylene-hexene copolymer. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and p.. |
|||
Puncture Energy | 3.73 J | 2.75 ft-lb | Dow Method |
Dow ELITE™ 5230G Enhanced Polyethylene Resin ™ 5230G is produced via INSITE™ Technology from Dow Plastics. It offers high impact strength and good puncture resistance at moderate stretch levels for irregularly shaped loads. In addition, th.. |