Polymer Property : Puncture Energy = 27.1 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 27.1 J
20.0 ft-lb
ASTM D3763-10
Topas Advanced Polymers TOPAS® IT X1 Cyclic Olefin Copolymer (COC)
TOPAS® IT X1 is an injection molding grade with heat and impact resistance. It is a moderately clear resin with high moisture barrier, chemical and heat resistance, making it suitable for products ..