Mechanical Properties Metric English Comments
Puncture Energy 37.0 J
27.3 ft-lb
Puncture Resistance @Max Load, 0°C; ASTM D3763
Eastman Provista MP001 Copolymer
Provista Copolymer MP001 is a resin specifically developed for extrusion into profiles where aesthetics such as high clarity and gloss, coupled with design flexibility, drive demand. Compared to com..
Puncture Energy 37.0 J
27.3 ft-lb
Puncture Resistance @Max Load, 0°C; ASTM D3763
Eastman Provista UVI Copolymer
Provista UVI is a Provista copolymer with an indoor/outdoor UV package added to prevent yellowing caused by light. Provista copolymer is a resin specifically developed for extrusion into profiles wh..
Puncture Energy 37.0 J
27.3 ft-lb
Puncture Resistance @Max Load, 0°C; ASTM D3763
Eastman Provista UVO Copolymer
Provista UVO is a Provista copolymer with an indoor/outdoor UV package added to prevent yellowing caused by light. Provista copolymer is a resin specifically developed for extrusion into profiles wh..