Mechanical Properties Metric English Comments
Puncture Energy 3.30 J
2.43 ft-lb
ASTM D3763
Chevron Phillips MarFlex® D139DK Metallocene Linear Low Density Polyethylene, Blown Film
This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du..
Puncture Energy 3.30 J
2.43 ft-lb
ASTM D3763
Chevron Phillips MarFlex® D139FK Metallocene Linear Low Density Polyethylene, Blown Film
This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du..
Puncture Energy 3.30 J

@Temperature -30.0 °C
2.43 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® BKV 35 H2.0 901510 Nylon 6, 35% Glass Fiber
PA 6, injection molding grade, 35% glass fibers, good heat-ageing resistanceApplication Examples: automotive structures
Puncture Energy 3.30 J

@Temperature -30.0 °C
2.43 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® BKV 35 H2.0 901510 Nylon 6, 35% Glass Fiber
PA 6, injection molding grade, 35% glass fibers, good heat-ageing resistanceApplication Examples: automotive structures