Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 4.00 J | 2.95 ft-lb | ISO 6603-2 |
Lanxess Durethan® BKV 140 H2.0 900051 Copolyamide, 40% Glass Fiber CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in.. |
|||
Puncture Energy | 4.00 J | 2.95 ft-lb | ISO 6603-2 |
Lanxess Durethan® BKV 15 000000 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers |
|||
Puncture Energy | 4.00 J @Temperature -30.0 °C |
2.95 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® BKV 230 H2.0 901510 Copolyamide, 30% Glass Fiber CoPA, injection molding grade, 30% glass fibers, elastomer-modified, higher impact and notched impact strength and also higher energy absorption under biaxial impact load than BKV 130, conditioning .. |
|||
Puncture Energy | 4.00 J @Temperature -30.0 °C |
2.95 ft-lb @Temperature -22.0 °F |
Conditioned; ISO 6603-2 |
Lanxess Durethan® BKV 230 H2.0 901510 Copolyamide, 30% Glass Fiber CoPA, injection molding grade, 30% glass fibers, elastomer-modified, higher impact and notched impact strength and also higher energy absorption under biaxial impact load than BKV 130, conditioning .. |
|||
Puncture Energy | 4.00 J @Temperature -30.0 °C |
2.95 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® DP 2131/20 H2.0 900051 Nylon 6, 20% Glass Fiber PA 6, injection molding grade, 20% glass fibers, better surface resistance to alcoholic calcium chloride-solution than BKV 20 H2.0, good heat-ageing resistance and weather resistance |
|||
Puncture Energy | 4.00 J @Temperature -30.0 °C |
2.95 ft-lb @Temperature -22.0 °F |
Conditioned; ISO 6603-2 |
Lanxess Durethan® DP 2131/20 H2.0 900051 Nylon 6, 20% Glass Fiber PA 6, injection molding grade, 20% glass fibers, better surface resistance to alcoholic calcium chloride-solution than BKV 20 H2.0, good heat-ageing resistance and weather resistance |
|||
Puncture Energy | 4.00 J @Temperature -30.0 °C |
2.95 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® DP 2131/20 W1 901317 Nylon 6, 20% Glass Fiber PA 6, injection molding grade, 20% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 20 H2.0, weather resistance, good heat-ageing resistance |
|||
Puncture Energy | 4.00 J @Temperature -30.0 °C |
2.95 ft-lb @Temperature -22.0 °F |
Conditioned; ISO 6603-2 |
Lanxess Durethan® DP 2131/20 W1 901317 Nylon 6, 20% Glass Fiber PA 6, injection molding grade, 20% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 20 H2.0, weather resistance, good heat-ageing resistance |
|||
Puncture Energy | 4.00 J | 2.95 ft-lb | ASTM 5748 |
Borealis Borstar® FB4230 LLDPE for Film Borstar FB4250T is a high molecular weight linear low density polyethylene grade combining good extrusion properties, excellent draw properties and good mechanical strength. Film made from Borstar .. |