Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 4.70 J | 3.47 ft-lb | Conditioned; ISO 6603-2 |
Lanxess Durethan® AKV 30 HR H2.0 901510 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, hydrolysis stabilized, good heat-ageing resistance |
|||
Puncture Energy | 4.70 J @Temperature -30.0 °C |
3.47 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® DP BKV 240 H2.0 901510 Copolyamide, 40% Glass Fiber CoPA, injection molding grade, 40% glass fibers reinforced, elastomer-modified, good heat-ageing resistance |
|||
Puncture Energy | 4.70 J @Temperature -30.0 °C |
3.47 ft-lb @Temperature -22.0 °F |
Conditioned; ISO 6603-2 |
Lanxess Durethan® DP BKV 240 H2.0 901510 Copolyamide, 40% Glass Fiber CoPA, injection molding grade, 40% glass fibers reinforced, elastomer-modified, good heat-ageing resistance |