Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 38.0 - 40.0 J | 28.0 - 29.5 ft-lb | Average value: 39.5 J Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |