Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 55.0 J | 40.6 ft-lb | Puncture Resistance @Max Load, 23°C; ASTM D3763 |
Eastman Eastalloy DA510 Polymer
(discontinued **) Eastalloy Polymer DA510 is a clear copolyester/polycarbonate alloy. This product has good physical properties. These include good impact strength, chemical resistance, heat resistance, dimensional s.. |
|||
Puncture Energy | 55.0 - 75.0 J @Temperature -30.0 - -30.0 °C |
40.6 - 55.3 ft-lb @Temperature -22.0 - -22.0 °F |
Average value: 66.4 J Grade Count:14 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Puncture Energy | 55.0 - 60.0 J @Temperature -30.0 - -30.0 °C |
40.6 - 44.3 ft-lb @Temperature -22.0 - -22.0 °F |
Average value: 56.5 J Grade Count:10 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
Puncture Energy | 55.0 - 70.0 J @Temperature -30.0 - -30.0 °C |
40.6 - 51.6 ft-lb @Temperature -22.0 - -22.0 °F |
Average value: 64.7 J Grade Count:16 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
Puncture Energy | 55.0 - 58.0 J @Temperature -30.0 - -30.0 °C |
40.6 - 42.8 ft-lb @Temperature -22.0 - -22.0 °F |
Average value: 57.0 J Grade Count:8 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Puncture Energy | 55.0 J @Temperature -40.0 °C |
40.6 ft-lb @Temperature -40.0 °F |
Puncture Resistance at Max Load; ISO 6603-2 |
Eastman DuraStar DS2000 Polymer, Natural Durastar DS2000 polymer has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. DS2000 has ver.. |
|||
Puncture Energy | 55.0 J @Temperature -40.0 °C |
40.6 ft-lb @Temperature -40.0 °F |
Puncture Resistance at Max Load; ISO 6603-2 |
Eastman DuraStar DS2110UVI Polymer, Natural Durastar DS2110UVI polymer, contains an ultraviolet light stabilization package. It is recommended for indoor applications requiring enhanced color stability upon extended exposure to fluorescent li.. |
|||
Puncture Energy | 55.0 J @Temperature -40.0 °C |
40.6 ft-lb @Temperature -40.0 °F |
Puncture Resistance at Max Load; ISO 6603-2 |
Eastman DuraStar MN621 Polymer, Natural Durastar Polymer MN621 was developed for the medical device industry and contains a mold release It processes easily and requires minimal drying time. It has superior toughness, high clarity and goo.. |
|||
Puncture Energy | 55.0 J @Temperature -40.0 °C |
40.6 ft-lb @Temperature -40.0 °F |
Puncture Resistance at Max Load; ISO 6603-2 |
Eastman Eastar BR203 Copolyester Eastar BR203 Copolyester contains a mold release additive. It has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilitie.. |
|||
Puncture Energy | 55.0 J | 40.6 ft-lb | ISO 6603-2 |
Covestro Apec® 1695 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=158 °CPreprocessingMax. Water content |
|||
Puncture Energy | 55.0 J | 40.6 ft-lb | ISO 6603-2 |
Covestro Apec® 1795 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=173°CPreprocessingMax. Water content |
|||
Puncture Energy | 55.0 J | 40.6 ft-lb | ISO 6603-2 |
Covestro Apec® 1895 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=183 °CPreprocessingMax. Water content |
|||
Puncture Energy | 55.0 J | 40.6 ft-lb | ISO 6603-2 |
Covestro Apec® 1897 Polycarbonate Easy flowingeasy to demoldUV-stabilizedsoftening temperature (VST/B 120)=182 °CPreprocessingMax. Water content |
|||
Puncture Energy | 55.0 J | 40.6 ft-lb | ISO 6603-2 |
Covestro Apec® 2097 Polycarbonate Easy flowingeasy to demoldUV-stabilizedsoftening temperature (VST/B 120)=202 °CPreprocessingMax. Water content |
|||
Puncture Energy | 55.0 J @Temperature -30.0 °C |
40.6 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® 1837* Polycarbonate, Impact Grade ISO 7391-PC,MP,(,,)-09-9Global gradeFormerly Makrolon DP1-1837MVR (300 °C/1.2 kg) 11 cm3/10 minImpact modifiedMedium viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable.. |
|||
Puncture Energy | 55.0 J @Temperature -30.0 °C |
40.6 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® 1899* Polycarbonate, Impact Grade Formerly Makrolon DP1-1899MVR (300 °C/1.2 kg) 15.5 cm³/10 minspecial flame retardant systemUL 94V-0/0.75 mmImpact modifiedMedium viscosityEasy releaseVicat softening temperature 50 N; 50 °C/h = 1.. |
|||
Puncture Energy | 55.0 J | 40.6 ft-lb | ISO 6603-2 |
Covestro Makrolon® 2467 Polycarbonate ISO 7391-PC,MFLR,(,,)-18-9Global gradeFormerly Makrolon DP1-1870MVR (300 °C/1.2 kg) 19 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmLow viscosityUV stabilizedEasy r.. |
|||
Puncture Energy | 55.0 J @Temperature -30.0 °C |
40.6 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® 6265 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minFlame retardantUL 94V-0/1.5 mmLow viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in opaque co.. |
|||
Puncture Energy | 55.0 J @Temperature -30.0 °C |
40.6 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® 6585 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFlame retardantUL 94V-0/1.2 mm5VA/3.0 mm and 5VB (WT) /2.0 mmHigh viscosityEasy releaseInjection molding - Melt temperature 28.. |
|||
Puncture Energy | 55.0 J | 40.6 ft-lb | ISO 6603-2 |
Covestro Makrolon® AL2447 Polycarbonate ISO 7391-PC,MLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minAutomotive lightingLow viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in transpa.. |
|||
Puncture Energy | 55.0 J @Temperature -30.0 °C |
40.6 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® LED2045 Polycarbonate ISO 7391-PC,MRT,(,,)-24-9Global gradeMVR (250 °C/2.16 kg) 16.5 cm3/10minLight guidesPC with highest transmissionLow viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable .. |
|||
Puncture Energy | 55.0 J | 40.6 ft-lb | ISO 6603-2 |
Covestro Makrolon® T7855 Polycarbonate, Impact Grade ISO 7391-PC,MPR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12 cm3/10 minImpact modifiedMedium viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in opaque colors onlyPre.. |
|||
Puncture Energy | 55.0 J | 40.6 ft-lb | ISO 6603-2 |
Covestro Makrolon® WB1239 Polycarbonate ISO 7391-PC,B,(,,)-05-9Global gradeMVR (300 °C/1.2 kg) 2.5 cm3/10 minBlow moldingHigh viscosityBranchedFood contact qualityExtrusion blow moldingInjection stretch blow moldingAvailable in transpare.. |
|||
Puncture Energy | 55.0 J @Temperature -30.0 °C |
40.6 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makroblend® DP UT3905 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendhigh flowimpact modifiedeasy releaseinjection molding grade Makroblend DP UT3905* offers superior flowability, good impact strength and excellent chemical resist.. |
|||
Puncture Energy | 55.0 J | 40.6 ft-lb | ISO 6603-2 |
Covestro Makrolon® 1248 Polycarbonate, Impact Grade ISO 7391-PC,MP,(,,)-09-9Formerly Makrolon KU1-1248MVR (300 °C/1.2 kg) 7.0 cm3/10 minFood contact qualityMedium viscosityImpact modifiedInjection molding - Melt temperature 280 - 320 °CAvailable in.. |
|||
Puncture Energy | 55.0 J @Temperature -30.0 °C |
40.6 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® 1260 Polycarbonate, Impact Grade ISO 7391-PC,MPR,(,,)-24-9Global gradeMVR (300 °C/1.2 kg) 34 cm3/10 minImpact modifiedLow viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in light colors onlyPreproc.. |
|||
Puncture Energy | 55.0 J | 40.6 ft-lb | ISO 6603-2 |
Covestro Makrolon® 2456 Polycarbonate ISO 7391-PC,MR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minFood contact qualityLow viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAvailab.. |
|||
Puncture Energy | 55.0 J @Temperature -30.0 °C |
40.6 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® 6487 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minFlame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmMedium viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 2.. |
|||
Puncture Energy | 55.0 J | 40.6 ft-lb | ISO 6603-2 |
Covestro Makrolon® DP1-1825* Polycarbonate, Impact Grade Developmental productISO 7391-PC,MP,(,,)-09-9MVR (300 °C/1.2 kg) 6.0 cm3/10 minImpact modifiedHigh viscosityInjection molding - Melt temperature 280 - 320 °CAvailable in opaque colors onlyPreproce.. |
|||
Puncture Energy | 55.0 J @Temperature -30.0 °C |
40.6 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® OD2015 Polycarbonate Global gradeOptical storage mediaLow viscosityEasy releaseHigh purityInjection moldingAvailable in natural color onlyPreprocessingMax. Water content |