Mechanical Properties Metric English Comments
Puncture Energy 75.0 J

@Temperature -30.0 °C
55.3 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 3206 Polycarbonate
ISO 7391-PC,M,(,,)-05-9MVR (300 °C/1.2 kg) 4.0 cm3/10 minFood contact qualityHigh viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtrusionAvailable in transpar..