Puncture Energy 90.0 J

@Temperature -30.0 °C
66.4 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® BC 40 SR2 000000 Nylon 6
PA 6 injection molding grade, high viscosity, non-reinforced, higher notched impact strength than BC 30, impact-modified
Puncture Energy 90.0 J

@Temperature -30.0 °C
66.4 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® BC 40 SR2 000000 Nylon 6
PA 6 injection molding grade, high viscosity, non-reinforced, higher notched impact strength than BC 30, impact-modified