Mechanical Properties Metric English Comments
Puncture Energy 10.0 - 10.0 J

@Temperature -30.0 - -30.0 °C
7.38 - 7.38 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 10.0 J Grade Count:1
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..