Polymer Property : Puncture Energy = 70.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 70.0 J

@Temperature -30.0 °C
51.6 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® B 31 SK 000000 Nylon 6
PA 6, injection molding grade, non-reinforced, easy flow, easy-release, rapid solidification, crystallizes somewhat more finely and uniformly than B 30 S
Puncture Energy 70.0 J

@Temperature -30.0 °C
51.6 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® B 31 SK 000000 Nylon 6
PA 6, injection molding grade, non-reinforced, easy flow, easy-release, rapid solidification, crystallizes somewhat more finely and uniformly than B 30 S
Puncture Energy 70.0 J
51.6 ft-lb
Puncture Resistance @ max load, -10°C; ISO 6603-2
Eastman Spectar® 14471 Copolyester
Spectar copolyester extrudes into plastic sheet that is sparkling clear, tough, chemically resistant, odor-free, versatile, easy to work with and affordable. Its toughness allows fabricators to use ..
Puncture Energy 70.0 J

@Temperature -30.0 °C
51.6 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 1804 Polycarbonate
MVR (300 °C/1.2 kg) 6.0 cm3/10 minhigh viscosityUV stabilizedoptimized for low plate-outimproved flammabilityUL 94 V-2/1.5 mm and 3.0 mmavailable in transparenttranslucent and opaque colorssolid sh..
Puncture Energy 70.0 J

@Temperature -30.0 °C
51.6 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 3103 MAS157 Polycarbonate
ISO 7391-PC,EL,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minExtrusionHigh viscosityUV stabilizedAvailable in color code 550115 onlySolid sheetCorrugated sheetPreprocessingMax. Water conte..
Puncture Energy 70.0 J

@Temperature -30.0 °C
51.6 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 3106 Polycarbonate
ISO 7391-PC,M,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFood contact qualityHigh viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtrusionAvailable..
Puncture Energy 70.0 J

@Temperature -30.0 °C
51.6 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 3107 Polycarbonate
ISO 7391-PC,MLR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minGeneral purposeHigh viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in transpare..
Puncture Energy 70.0 J

@Temperature -30.0 °C
51.6 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 3156 Polycarbonate
ISO 7391-PC,MR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFood contact qualityHigh viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtru..
Puncture Energy 70.0 J
51.6 ft-lb
Puncture energy -30°C
Covestro Makrolon® 3158 Polycarbonate
Key Features:Release agentUnfilledSuitable processing methods:Injection moldingExtrusionBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated..
Puncture Energy 70.0 J

@Temperature -30.0 °C
51.6 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® DP1-1821* Polycarbonate
Developmental productMVR (300 °C/1.2 kg) 6.0 cm3/10 minHigh viscosityUV stabilizedEasy releaseInjection moldingAvailable in colorless transparent onlyPreprocessingMax. Water content
Puncture Energy 70.0 J

@Temperature -30.0 °C
51.6 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® LQ3147 Polycarbonate
ISO 7391-PC,MLR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minOptical lensHigh viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in clear tints ..
Puncture Energy 70.0 J

@Temperature -30.0 °C
51.6 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® LTG3123 Polycarbonate
PreprocessingMax. Water content
Puncture Energy 70.0 J

@Temperature -30.0 °C
51.6 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® Rx1805 Polycarbonate
ISO 7391-PC,M,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minMedical devicesLipid resistantsuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modifie..
Puncture Energy 70.0 J

@Temperature -30.0 °C
51.6 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® Rx2430 Polycarbonate
ISO 7391-PC,M,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minMedical devicessuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modified ISO 10993-1 an..
Puncture Energy 70.0 J

@Temperature -30.0 °C
51.6 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® LQ3187 Polycarbonate
ISO 7391-PC,MLR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minOptical lensHigh viscosityUV stabilizedUV 400 cut offEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable i..
Puncture Energy 70.0 J

@Temperature -30.0 °C
51.6 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® Rx2530 Polycarbonate
ISO 7391-PC,M,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 14.5 cm3/10 minMedical devicessuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modified ISO 10993-1 ..
Puncture Energy 70.0 J

@Temperature -30.0 °C
51.6 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® KU1-1230* Polycarbonate
ISO 7391-PC,EFL,(,,)-09-9Developmental productMVR (300 °C/1.2 kg) 8.5 cm3/10 minFlame retardant16 mm Triple wall sheet/B1 classification (DIN 4102)Medium viscosityUV stabilizedExtrusionAs of 1 Sept..