Polymer Property : Torsional Stiffness = 160 MPa
Polymer Property :
Torsional Stiffness =
160 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Torsional Stiffness
160
MPa
23200
psi
DIN 53447
Fluorseals PTFE Unfilled
Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials.