Polymer Property : Torsional Stiffness = 279.81 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Torsional Stiffness 1.9292 MPa
279.81 psi
At 75°F (24°C); ASTM D1043
Advanced Polymer Alloys Alcryn® 1060 BK Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..