Torsional Stiffness 20.0 - 500 MPa
2900 - 72500 psi
Average value: 198 MPa Grade Count:11
Overview of materials for Polyester Thermoplastic Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values..
Torsional Stiffness 20.0 MPa
2900 psi
+20°C; ASTM D1043
C.O.I.M. LARIPUR® LPR5020 Standard Adipate Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..