Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Torsional Stiffness = 68500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Torsional Stiffness 472 MPa
68500 psi
-20°C; ASTM D1043
C.O.I.M. LARIPUR® LPR70D60 PTMG Polyether Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
Copyright © lookpolymers.com All Rights Reserved