Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Bearing Yield Strength | 566.1 MPa | 82110 psi | Pin Type (e/D = 2.0) |
IBC Advanced Alloys Beralcast® 310 Beryllium-Aluminum Alloy This alloy, a metal matrix composite, consisting of between 60 and 70% Be (by weight) is a wrought product offered by IBC Engineered Materials to be used in the process of manufacturing extrusions f.. |