Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Bearing Yield Strength | 848 MPa @Temperature 24.0 °C |
123000 psi @Temperature 75.2 °F |
Dry |
Hexcel® HexPly® F522 Epoxy Resin, W3C282 Carbon Fabric Hexcel designation: TW3C282-42"-F522; Fiber: Toho® G30/500-3KInformation provided by HexCel |