Polymer Property : Ultimate Bearing Strength = 2067 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ultimate Bearing Strength 2067 MPa
299800 psi
Transverse, pin diameter = 0.250 in. (6.35 mm). Edge distance ratio of 1.5.
Special Metals INCONEL® 706 Precipitation Hardening Alloy, Cold Rolled Sheet, 3 Part Heat Treatment, 0.062 inch (1.57 mm) Thickness
Tensile and bearing strengths (ultimate and yield) and elongation values reported here are typical for Cold Rolled Sheet, 3 Part Heat Treatment, 0.062 inch (1.57 mm) Thickness samples. Density and m..