Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Rupture = 0.000491 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 1.44e-7 - 0.000491 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000209 - 0.0711 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories INCT-100S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 1.44e-7 - 0.000491 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000209 - 0.0711 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories INCT-110S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 2.41e-7 - 0.000491 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000349 - 0.0711 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories INCT-120S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 1.44e-7 - 0.000491 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000209 - 0.0711 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories INCT-80N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 6.74e-8 - 0.000491 GPa

@Temperature 110 °C,
Time 86400 sec
0.00000977 - 0.0711 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories MIX-3 Light-Weight Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 3.37e-7 - 0.000491 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000489 - 0.0711 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories PT-150 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 3.37e-7 - 0.000491 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000489 - 0.0711 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories PT-160 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 3.37e-7 - 0.000491 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000489 - 0.0711 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories PT-140 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 3.37e-7 - 0.000491 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000489 - 0.0711 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories PAC-160 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 3.37e-7 - 0.000491 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000489 - 0.0711 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories PT-150 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).