Modulus of Rupture 0.000930 GPa

@Temperature 815 °C
0.135 ksi

@Temperature 1500 °F
ASTM C268
BNZ Materials Bazelite 2500 LI Insulating Castable
Blaz 2500 LI is an extremely strong insulating castable designed for general purpose use in those areas that require this combination of light weight and high strength, such as forge furnace doors a..