Mechanical Properties Metric English Comments
Modulus of Rupture 0.0014715 - 0.0034335 GPa

@Temperature 500 °C,
Time 10800 sec
0.21343 - 0.49799 ksi

@Temperature 932 °F,
Time 3.00 hour
Chosun Refractories INCT-110N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0014715 - 0.0024525 GPa

@Temperature 1000 °C,
Time 10800 sec
0.21343 - 0.35571 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories INCT-110S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0014715 - 0.0034335 GPa

@Temperature 500 °C,
Time 10800 sec
0.21343 - 0.49799 ksi

@Temperature 932 °F,
Time 3.00 hour
Chosun Refractories INCT-120N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0014715 - 0.0034335 GPa

@Temperature 1000 °C,
Time 10800 sec
0.21343 - 0.49799 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories INCT-120S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0014715 - 0.0034335 GPa

@Temperature 500 °C,
Time 10800 sec
0.21343 - 0.49799 ksi

@Temperature 932 °F,
Time 3.00 hour
Chosun Refractories INCT-135N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0014715 - 0.0044145 GPa

@Temperature 1000 °C,
Time 10800 sec
0.21343 - 0.64028 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories INCT135S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0014715 - 0.0044145 GPa

@Temperature 500 °C,
Time 10800 sec
0.21343 - 0.64028 ksi

@Temperature 932 °F,
Time 3.00 hour
Chosun Refractories INCT-140 Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0014715 - 0.0044145 GPa

@Temperature 1000 °C,
Time 10800 sec
0.21343 - 0.64028 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories INCT-140 Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0014715 - 0.0044145 GPa

@Temperature 1000 °C,
Time 10800 sec
0.21343 - 0.64028 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories INCT-160 Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0014715 - 0.0044145 GPa

@Temperature 1350 °C,
Time 10800 sec
0.21343 - 0.64028 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories INCT-170 Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).