Polymer Property : Modulus of Rupture = 0.006867 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.002943 - 0.006867 GPa

@Temperature 1000 °C,
Time 10800 sec
0.4269 - 0.9960 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories CT-140S Fireclay Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.006867 GPa

@Temperature 110 °C,
Time 86400 sec
0.4269 - 0.9960 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories HACT-165G High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.006867 GPa

@Temperature 1000 °C,
Time 10800 sec
0.4269 - 0.9960 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories HACT-165G High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.006867 GPa

@Temperature 110 °C,
Time 86400 sec
0.4269 - 0.9960 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories HACT-170 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.006867 GPa

@Temperature 1000 °C,
Time 10800 sec
0.4269 - 0.9960 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories HACT-170 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 9.62361e-7 - 0.006867 GPa

@Temperature 1000 °C,
Time 10800 sec
0.000139581 - 0.9960 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories SCX-90IP Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.001962 - 0.006867 GPa

@Temperature 1350 °C,
Time 10800 sec
0.2846 - 0.9960 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories HACT-150 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.006867 GPa

@Temperature 1350 °C,
Time 10800 sec
0.4269 - 0.9960 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories HACT-155 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.006867 GPa

@Temperature 110 °C,
Time 86400 sec
0.4269 - 0.9960 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories HACT-155 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.006867 GPa

@Temperature 1350 °C,
Time 10800 sec
0.4269 - 0.9960 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories HACT-165 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.002943 - 0.006867 GPa

@Temperature 110 °C,
Time 86400 sec
0.4269 - 0.9960 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories HACT-165 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).