Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00689 GPa @Temperature 1450 °C |
1.00 ksi @Temperature 2640 °F |
|
Zircar Ceramics DAHP Dense Alumina Hearth Plate ZIRCAR Dense Alumina Hearth Plates are used for supporting loads in high temperature furnaces and other thermal process systems. These dense plates are made of fully sintered fine grain high purity .. |