Mechanical Properties Metric English Comments
Modulus of Rupture 0.012753 GPa

@Temperature 1350 °C,
Time 10800 sec
1.8497 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories A40 Special High-Density Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.012753 GPa

@Temperature 1000 °C,
Time 10800 sec
1.8497 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories HSC-16SF-W2 Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.012753 GPa

@Temperature 1500 °C,
Time 10800 sec
1.8497 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories HSC-17 Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.012753 - 0.015696 GPa

@Temperature 1500 °C,
Time 10800 sec
1.8497 - 2.2765 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories PTF-180 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.012753 GPa

@Temperature 1350 °C,
Time 10800 sec
1.8497 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories SFC-165 High-Alumina Castable