Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00981 - 0.012753 GPa @Temperature 1350 °C, Time 10800 sec |
1.42 - 1.8497 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories PTC-165 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |