Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.016677 GPa @Temperature 1500 °C, Time 10800 sec |
2.4188 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories BLC Lance Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.016677 GPa @Temperature 1350 °C, Time 10800 sec |
2.4188 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories LPCT-17PI Lance Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.016677 GPa @Temperature 110 °C, Time 86400 sec |
2.4188 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories SFC-90SC High-Alumina Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |