Modulus of Rupture 0.024525 GPa

@Temperature 1000 °C,
Time 10800 sec
3.5571 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories HSC-16H Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.024525 GPa

@Temperature 1000 °C,
Time 10800 sec
3.5571 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories HSC-18RA Dense and High-Strength Castable, Superdense
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.024525 GPa

@Temperature 250 °C
3.5571 ksi

@Temperature 482 °F
Chosun Refractories SB50 Bricks, Oxide Bonded SiC
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.024525 GPa

@Temperature 250 °C
3.5571 ksi

@Temperature 482 °F
Chosun Refractories SC80 Bricks, Oxide Bonded SiC
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.024525 GPa

@Temperature 1400 °C
3.5571 ksi

@Temperature 2550 °F
Chosun Refractories SC80 Bricks, Oxide Bonded SiC
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.024525 GPa

@Temperature 1350 °C,
Time 10800 sec
3.5571 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories SFC-70 SiC Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.024525 GPa

@Temperature 1400 °C,
Time 10800 sec
3.5571 ksi

@Temperature 2550 °F,
Time 3.00 hour
Chosun Refractories SFC-90W High-Alumina Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.024525 GPa

@Temperature 1350 °C,
Time 10800 sec
3.5571 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories SFC-UL90S High-Alumina Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).