Polymer Property : Modulus of Rupture = 0.09960 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0001962 - 0.0006867 GPa

@Temperature 500 °C,
Time 10800 sec
0.02846 - 0.09960 ksi

@Temperature 932 °F,
Time 3.00 hour
Chosun Refractories INCT-80S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).