Polymer Property : Modulus of Rupture = 0.160 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00110 GPa

@Temperature 540 °C
0.160 ksi

@Temperature 1000 °F
Fired; ASTM C268
BNZ Materials Bazelite 2600 LI Insulating Castable
Blaz 2600 LI is s low iron, high purity castable for service to 2600°F (1427°C) in controlled atmosphere applications. Recommended for casting monolithic shapes and furnace liningsInformation prov..
Modulus of Rupture 0.00110 GPa

@Temperature 104 °C
0.160 ksi

@Temperature 219 °F
Dried; ASTM C268
BNZ Materials Bazelite 2100 Insulating Castable
Blaz 2100 is a general purpose lightweight castable for use as an exposed hot face refractory or as a very thermally efficient back-up to a dense refractory lining. Can be installed by casting, gunn..
Modulus of Rupture 0.00110 GPa

@Temperature 540 °C
0.160 ksi

@Temperature 1000 °F
Fired; ASTM C268
BNZ Materials Bazelite 2500 LI Insulating Castable
Blaz 2500 LI is an extremely strong insulating castable designed for general purpose use in those areas that require this combination of light weight and high strength, such as forge furnace doors a..