Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00200 GPa @Temperature 538 °C |
0.290 ksi @Temperature 1000 °F |
|
Pyrotek Pyrocast 80 Lightweight Castable Refractory Pyrocast 80 is a lightweight, low cement, fused silica castable designed for moderate flow molten aluminum contact applications. Pyrocast 80 offers low thermal conductivity, excellent resistance to.. |
|||
Modulus of Rupture | 0.00200 GPa @Temperature 816 °C |
0.290 ksi @Temperature 1500 °F |
|
Pyrotek Pyrocast 80 Lightweight Castable Refractory Pyrocast 80 is a lightweight, low cement, fused silica castable designed for moderate flow molten aluminum contact applications. Pyrocast 80 offers low thermal conductivity, excellent resistance to.. |
|||
Modulus of Rupture | 0.00200 GPa @Temperature 1371 °C |
0.290 ksi @Temperature 2500 °F |
ASTM C268 |
BNZ Materials Bazelite 2500 LI Insulating Castable Blaz 2500 LI is an extremely strong insulating castable designed for general purpose use in those areas that require this combination of light weight and high strength, such as forge furnace doors a.. |