Mechanical Properties Metric English Comments
Modulus of Rupture 0.00210 GPa

@Temperature 540 °C
0.305 ksi

@Temperature 1000 °F
Fired; ASTM C268
BNZ Materials Blazecrete 2500 HS Dense Castable
Blazecrete 2500 HSis a high-duty castable designed to withstand loads and resist normal abrasion and erosion at moderate temperatures to 2500°F (1371°C). Use with Blaz 2100 for a dual component li..
Modulus of Rupture 0.00210 GPa

@Temperature 815 °C
0.305 ksi

@Temperature 1500 °F
ASTM C268
BNZ Materials Blazecrete 2500 HS Dense Castable
Blazecrete 2500 HSis a high-duty castable designed to withstand loads and resist normal abrasion and erosion at moderate temperatures to 2500°F (1371°C). Use with Blaz 2100 for a dual component li..
Modulus of Rupture 0.00210 GPa

@Temperature 1260 °C
0.305 ksi

@Temperature 2300 °F
ASTM C268
BNZ Materials Blazecrete 2500 HS Dense Castable
Blazecrete 2500 HSis a high-duty castable designed to withstand loads and resist normal abrasion and erosion at moderate temperatures to 2500°F (1371°C). Use with Blaz 2100 for a dual component li..
Modulus of Rupture 0.00210 GPa

@Temperature 540 °C
0.305 ksi

@Temperature 1000 °F
Fired; ASTM C268
BNZ Materials Blazecrete 2300 ARG Dense Castable
Blazecrete 2300 ARG is an alumina-silica castable with high strength and abrasion resistance. For service to 2300°F (1260°C). May be gunned or slap-troweled over Blaz 2000G to obtain a high streng..
Modulus of Rupture 0.00210 GPa

@Temperature 815 °C
0.305 ksi

@Temperature 1500 °F
ASTM C268
BNZ Materials Blazecrete 2300 ARG Dense Castable
Blazecrete 2300 ARG is an alumina-silica castable with high strength and abrasion resistance. For service to 2300°F (1260°C). May be gunned or slap-troweled over Blaz 2000G to obtain a high streng..
Modulus of Rupture 0.00210 GPa

@Temperature 1260 °C
0.305 ksi

@Temperature 2300 °F
ASTM C268
BNZ Materials Blazecrete 2300 ARG Dense Castable
Blazecrete 2300 ARG is an alumina-silica castable with high strength and abrasion resistance. For service to 2300°F (1260°C). May be gunned or slap-troweled over Blaz 2000G to obtain a high streng..