Mechanical Properties Metric English Comments
Modulus of Rupture 0.02943 GPa

@Temperature 1000 °C,
Time 10800 sec
4.269 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories HSC-18SC Dense and High-Strength Castable, Superdense
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.02943 GPa

@Temperature 250 °C
4.269 ksi

@Temperature 482 °F
Chosun Refractories SB65S Bricks, Oxide Bonded SiC
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.02943 GPa

@Temperature 1400 °C
4.269 ksi

@Temperature 2550 °F
Chosun Refractories SB75 Bricks, Oxide Bonded SiC
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.02943 GPa

@Temperature 250 °C
4.269 ksi

@Temperature 482 °F
Chosun Refractories SB85S Bricks, Oxide Bonded SiC
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.02943 GPa

@Temperature 250 °C
4.269 ksi

@Temperature 482 °F
Chosun Refractories SB90S Bricks, Oxide Bonded SiC
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.02943 GPa

@Temperature 250 °C
4.269 ksi

@Temperature 482 °F
Chosun Refractories SBSN20 Nozzle
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).