Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | >= 40.0 kN/m | >= 228 pli | ASTM D624 |
Multibase Multi-Flex® TPE G 7455 S BLK The burn rate is 0 in/min (0 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 40.0 kN/m | 228 pli | Die B,post cured- 2 hours at 200°C; ASTM D624 |
Multibase SILASTIC® 7-6830 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Tear Strength | 40.0 kN/m | 228 pli | ISO 34-1 |
PolyOne OnFlex™ S HF 90A-3S1988 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
Tear Strength | >= 40.0 kN/m | >= 228 pli | Method B; ISO 34 |
S&E Specialty Polymers SE900-6 PVC Description: PVC weatherable, integral colored, filledApplications: Roof Ditch Molding Skin which meets the Ford WSKM4D689-A5Information provided by S&E Specialty Polymers |
|||
Tear Strength | 40.0 kN/m | 228 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 4.0 PHR MBTS MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | ISO 34B |
Huntsman AVALON® 60 AE-ESD Thermoplastic Polyurethane AVALON® ESD range are soft TPUs that deliver the improved bonding strength and mechanical properties required to produce high-quality footwear on roundtable machines – specifically safety sh.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | ISO 34B |
Huntsman AVALON® 65 AK-ESD Thermoplastic Polyurethane AVALON® ESD range are soft TPUs that deliver the improved bonding strength and mechanical properties required to produce high-quality footwear on roundtable machines – specifically safety sh.. |
|||
Tear Strength | >= 40.0 kN/m | >= 228 pli | DIN 53507 |
Karina 75/200 Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | 40.0 kN/m | 228 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2640 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 3286/50 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 3486/50 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Tear Strength | >= 40.0 kN/m | >= 228 pli | DIN 53507 |
Karina CAK 75-48/1 Black PVC Compound Reclaimed PVC compound recommended for soles injectionInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | 40.0 kN/m | 228 pli | Die B |
Momentive Performance Materials TUFELâ„¢ II 94406 Low Volatile Extrusion Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | MD; ISO 6383-2 |
Iran Petrochemical (PCC) LS0085/KJ Low Density Polyethylene LS0085/KJ is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.Application: shrink packaging.Information prov.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | |
Shin-Etsu Silicones LIMSâ„¢ KE1950-50A/B Elastomer KE-1950-50 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy .. |
|||
Tear Strength | 40.0 kN/m | 228 pli | DIN 53515 |
Lubrizol ESTANE® T5275 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 40.0 kN/m | 228 pli | ASTM D2240 |
UBE UBEPOL BR340L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
Tear Strength | 40.0 kN/m | 228 pli | |
Trelleborg R698 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 40.0 kN/m | 228 pli | |
Trelleborg R798 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 40.0 kN/m | 228 pli | GB/T 529 |
Chengdu Polyster 6500 General Grade TPV Information provided by Chengdu Polyster Co., Ltd. |
|||
Tear Strength | 40.0 kN/m | 228 pli | ASTM D624 |
ELASTO UK Dryflex® 502800S SEBS Based Material, Unfilled Qualities, 80A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | DIN ISO 34-1/Bb |
BASF Elastollan S 50 A SPF TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | DIN ISO 34-1/Bb |
BASF Elastollan SP 9213 TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Tear Strength | >= 40.0 kN/m | >= 228 pli | ISO 34 |
Austin Novel Materials Texalan® 365A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |
|||
Tear Strength | 40.0 kN/m | 228 pli | Die B |
Momentive Performance Materials Silopren™ LSR 3386/30 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | Die C; ASTM D412 |
Alliance Polymers Zythane™ 4070A Thermoplastic Polyurethane Elastomer Zythane™ 4070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tear Strength | 40.0 kN/m | 228 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.5 PHR Thanecure® ZM MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 4.0 PHR MBTS MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |