Material Notes:
Description: PVC weatherable, integral colored, filledApplications: Roof Ditch Molding Skin which meets the Ford WSKM4D689-A5Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity <= 1.35 g/cc
<= 1.35 g/cc
ASTM D792, A
Mechanical Properties Metric English Comments
Hardness, Shore A 70 - 80

@Time 15.0 sec
70 - 80

@Time 0.00417 hour
ASTM D2240
Tensile Strength >= 11.0 MPa
>= 1600 psi
Type IV, 500mm/min; ASTM D638
Elongation at Break >= 240 %
>= 240 %
Type IV, 500mm/min; ASTM D638
Tear Strength >= 40.0 kN/m
>= 228 pli
Method B; ISO 34
Descriptive Properties Value Comments
Accelerated Weathering <3.0 DE
after 2000 kj/m<sup>2</sup>, SAEJ2527
Cold Flex -30°C
FLTM BN 102-01
Users viewing this material also viewed the following: