Mechanical Properties Metric English Comments
Tear Strength 0.0700 kN/m
0.399 pli
ASTM D 624
Eurofoam Porocell POR 304 CM-OPC EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.