Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 0.430 kN/m | 2.45 pli | ASTM D 624 |
Eurofoam Porocell POR 303/B GR CR-Neoprene/NBR Foam Polychloroprene and acrylonitrile butadiene foam rubber. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam.. |
|||
Tear Strength | 0.430 kN/m | 2.45 pli | ASTM D 624 |
Eurofoam Porocell POR 303/B RS CR-Neoprene/NBR Foam Polychloroprene and acrylonitrile butadiene foam rubber. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam.. |
|||
Tear Strength | 0.430 kN/m | 2.45 pli | ASTM D 624 |
Eurofoam Porocell POR 303/B CR-Neoprene/NBR Foam Polychloroprene and acrylonitrile butadiene foam rubber. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam.. |