Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 0.540 kN/m | 3.08 pli | Die C; ASTM D624 |
Covestro Bayfit® SA Polyurethane Sound Absorbing Foam, High-Resilience, Higher density Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Tear Strength | 0.540 kN/m | 3.08 pli | Die C; ASTM D624 |
Covestro Bayfit® SA Polyurethane Sound Absorbing Foam, Viscoelastic Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |