Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 1.12 kN/m | 6.40 pli | Die "C", average; ASTM D3574 |
Lendell Nolatex® Latex Free Foam This foam is used in the cosmetics industry and also possesses insulation qualities.Applications:Cosmetic Wedges and Puffs, Padding, High Insulative Value Applications, Makovers ® Disposable Make.. |