Polymer Property : Tear Strength = 1.20 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 1.20 kN/m
6.85 pli
BS EN ISO 8067 1995
Zotefoams Plastazote® LD45FR Low Density Polyethylene Foam, Flame Retardant
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Tear Strength 1.20 kN/m
6.85 pli
Die C; ASTM D624
Covestro Bayfill® 380 Polyurethane Semi-Rigid Foam, Polymeric Catalyst, Open Pour, MDI-based 2-Component Liquid System
Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Tear Strength 1.20 kN/m
6.83 pli
3M 12049 Black 3/8" (9.5 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Tear Strength 1.20 kN/m
6.83 pli
3M 12050 Black 1/2" (12.7 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Tear Strength 1.20 kN/m
6.83 pli
3M 12062 Black 3/32" (2.4 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Tear Strength 1.20 kN/m
6.83 pli
3M 12046 Black 1/16" (1.6 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Tear Strength 1.20 kN/m
6.83 pli
3M 12048 Black 1/8" (3.2 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Tear Strength 1.20 kN/m
6.83 pli
3M 12054 Black 1/4" (6.4 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Tear Strength 1.20 kN/m
6.83 pli
3M 12056 Black 3/16" (4.8 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..