Mechanical Properties Metric English Comments
Tear Strength 1.31 kN/m
7.50 pli
Split; ASTM D624
Northstar Polymers MPP-V37A Polyurethane Gel Elastomer
This two-component polyurethane casting system makes type of soft elastomer material known as “gel”. Applications for this material include filling component for computer keyboard/mouse-pad wrist..