Mechanical Properties Metric English Comments
Tear Strength 0.240 kN/m
1.37 pli
ASTM D 624
Eurofoam Evacell XM 2001 EVA + PE Foam
Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di..