Mechanical Properties Metric English Comments
Tear Strength >= 0.265 kN/m
>= 1.51 pli
Bond strength between laminate layers; ASTM F88F88M
OCTAL DPET™/PE Laminate Sheet with Improved Barrier Properties
Clear direct-to-sheet amorphous PET sheet with a polyethylene laminate film. Approved for food contact packaging. Information provided by OCTAL Petrochemicals.
Tear Strength >= 0.265 kN/m
>= 1.51 pli
Bond strength between laminate layers; ASTM F88F88M
OCTAL DPET™/PE Lock-Up Laminate Sheet
Clear direct-to-sheet amorphous PET sheet with a polyethylene laminate film. Approved for food contact packaging. Information provided by OCTAL Petrochemicals.
Tear Strength >= 0.265 kN/m
>= 1.51 pli
Bond strength between laminate layers; ASTM F88F88M
OCTAL DPET™/PE Peelable Laminate Sheet
Clear direct-to-sheet amorphous PET sheet with a polyethylene laminate film. Approved for food contact packaging. Information provided by OCTAL Petrochemicals.