Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 1.59 kN/m | 9.07 pli | JIS K6301-B |
Stellarchem LP-855 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Tear Strength | 1.59 kN/m | 9.07 pli | BS EN ISO 8067 1995 |
Zotefoams Evazote® VA65 Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |